Refractoriness under load (RUL) of fireclay bricks (under a load of 2 kg/cm2 ) is __________ °C.
500
1000
>1350
>2000
Correct Answer:
>1350
← Previous Question
Next Question→
More Questions from
Refractory Technology
Which of the following is not a high alumina refractory material?
Porosity of fireclay refractories is __________ percent.
Which one contains minimum percentage of SiO2?
Zirconia refractories are not used in
With decrease in porosity, the __________ of the refractories decreases.
An ideal refractory should have high
Highest melting (m.p = 3070°C) oxide refractory is
SiO2 percentage in firebrick is about
Maximum apparent porosity of magnesite bricks is about __________ percent.
Mullite is chemically represented by
Discussion & Comments
No comments yet. Be the first to comment!
Name:
Comment:
Post Comment
Join Discussion
Discussion & Comments